A tile comes out of the kiln with a lighter line running along its whole length, and suspicion immediately falls on the printhead. Sometimes that is right. Other times the cause is an ink that has settled, a glaze that absorbs unevenly or a firing cycle that has shifted the shade, and cleaning the printheads changes nothing.

A digital printing defect is the visible trace of a variable that has changed at some point in the chain formed by the machine, the ink, the surface and the kiln. Reducing it requires locating that point first and acting on it afterwards, not the other way round.

Which defects appear most often in digital ceramic printing?

On the line, a defect is recognised by its appearance long before its cause. The table brings together the six that recur most, how they are identified and where they tend to originate, so that it serves as a map before going into each one.

Defect How to recognise it Where it usually originates
Banding and lines Lighter or darker stripes parallel to the direction of travel, repeated on every piece Printhead and nozzles; coarse particles in the ink; air in the circuit
Lack of density Pale colour across the whole design or in a single channel Ink viscosity and temperature, batch, printhead wear, absorption of the surface
Lack of definition and satellite drops Blurred outlines and stray dots around the shapes Distance to the substrate, surface tension of the ink
Misalignment and stitching marks Colour halos; narrow band between two adjacent printheads Synchronisation, alignment of modules and printheads, pieces out of square
Shade variations Differences between pieces, between batches or between areas of a piece Ink batch, glaze weight, firing cycle, calibration
Pinholes in the printed area Dots, craters or matt areas only where there is ink Ink load, evacuation of organic matter, firing cycle

How can you tell at which point in the process the defect originates?

The question that organises the diagnosis is where in the process the defect begins. Four checks make it possible to answer without dismantling anything.

Does it appear before or after the kiln?

Take a printed piece out before it enters the kiln and examine it in good light, preferably raking light. If the defect is already there, the cause lies between the printer, the ink and the surface that receives it. If the piece comes out clean and the problem appears after firing, check the glaze, the ink load and the kiln.

There is a nuance: the pigment does not show its final shade until firing. In the raw state, differences in density, banding and lack of definition can be seen, but a shift in shade is only confirmed after the kiln.

Where does it repeat?

The position of the defect on the piece already points to the cause. A line fixed at the same point across the width points to a specific nozzle or printhead. A variation that changes with each batch points to the ink. A stripe of a different shade always on the same side points to a temperature difference across the width of the kiln. And a defect that appears only in one area of the design, or only on a particular glaze, points to the surface.

When did it start?

Note what changed just before the first defect: a new ink batch, a new glaze or engobe, a stop with cleaning, the replacement of a printhead, a change to the firing cycle. The cause is usually among the changes of the last hours or days, not in the rest of the process.

How to test the hypothesis

Once identified, change one variable at a time and compare the result with a reference piece or “banding” print made under known conditions. If you change the ink batch and clean the printheads at the same time, you will not know which of the two actions solved the problem, and the defect will come back without explanation.

How can banding and lines be avoided in inkjet printing?

In industrial ceramic decoration, single-pass printing is the usual approach: the piece moves under fixed modules of piezoelectric printheads and each nozzle always prints the same line. If a nozzle fails, the defect is repeated on every piece until it is corrected. That is why bands or streaks are the defect that is recognised fastest and, often, the first one to rule out.

Blocked or deviated nozzles, and air in the circuit

A blocked nozzle does not eject ink and leaves a light line. A deviated nozzle does eject, but the drop leaves at an angle and lands out of place, leaving a light line next to a darker one. The deviation is usually due to dirt, dried ink or wear on the nozzle plate.

The third case is air. After refilling a tank, changing a filter or purging the circuit, bubbles can remain that interrupt ejection from a printhead or several nozzles. If the fault appears right after one of those interventions, start there.

Cleaning, filters and stoppages

Ceramic inks lose vehicle through evaporation when the printhead is left stopped and uncapped. Ink that dries on the nozzle plate ends up blocking the nozzles or deviating the drop. That is why it is advisable to cap the printheads during stoppages and follow the cleaning and purging procedure indicated by the manufacturer.

The circuit filters retain coarse particles and agglomerates. A saturated filter reduces the flow of ink reaching the printhead and causes ejection failures, so it should be changed according to the manufacturer's schedule and not wait until lines appear. Dust on the line completes the list of causes: a closed, clean cabinet keeps it from reaching the nozzle plate.

Printhead wear

A printhead gradually loses nozzles with working hours. Some machines compensate for a failed nozzle with the adjacent ones, and as long as that compensation goes unnoticed the line keeps producing. When the number of faulty nozzles grows, it stops going unnoticed. Keep a record of the nozzle map of each printhead and set a replacement criterion, so that the change is decided with data.

Distance to the substrate and firing parameters

A lack of definition usually comes from the distance between the printhead and the surface. The greater it is, the further the drop travels and the more its point of impact is scattered, so the outline loses sharpness. Satellite drops, those stray dots around the shapes, are related to the ejection speed and the surface tension of the ink, and are usually corrected by adjusting the printhead parameters.

These parameters, voltage and waveform, are calibrated for each ink. If you change ink or reference without recalibrating, the drop changes in volume and speed, and the defect appears even though the printheads are in perfect condition.

Synchronisation and module alignment

Misalignment between colours originates in synchronisation. If the belt speed is not constant or the feed reading fails, each module prints at a different point and the channels stop coinciding, with colour halos around the shapes. After replacing a printhead or a module, it must be realigned before production.

On printers with several printheads per module, the stitching mark also appears: a narrow band in the area where two adjacent printheads overlap. It is due to a poorly adjusted overlap or to differences in ejection between the two, and it is corrected by aligning and calibrating the printheads that form it. Pieces that are out of square or enter crooked make both defects worse, so it is advisable to check the entry guides as well.

How does the ink influence printing defects?

Ceramic inkjet inks are suspensions of inorganic pigments finely dispersed in a liquid vehicle, and defects appear when that suspension stops behaving as the printhead expects. Three properties define it: particle size and dispersion, viscosity and surface tension. In our digital inks we work with average particle sizes below 1 µm, a viscosity of 8-15 mPa·s at 25 °C and a surface tension of 25-35 mN/m, and we control those parameters during manufacturing. The comparison between pigment-based inks and encapsulated pigments explains how each technology shapes the formulation.

Particle size and sedimentation

One large particle or an agglomerate is enough to block a nozzle, which is why the particle size distribution matters as much as the average size. At rest, particles tend to settle: the first volume of ink reaching the printhead after a long stoppage may have a different pigment concentration, with a corresponding effect on shade and on the nozzles. Follow the tank agitation and recirculation guidelines and do not load an ink with visible sediment at the bottom without first consulting your supplier.

Viscosity and working temperature

The printhead needs a stable viscosity to always form the same drop, which is why the circuit keeps the ink at a controlled temperature. If the working temperature drifts, the viscosity, the drop volume and, with them, the colour density and the sharpness of the outline change.

Surface tension and nozzle plate

Surface tension regulates how the drop forms as it leaves and how it wets the nozzle plate. An ink that wets the plate excessively leaves a film around the nozzles, and that film can deviate the following drops.

Batch changes, mixtures and effect inks

Mixing an ink with remnants of another reference can alter its behaviour in the printhead, so it is advisable to empty and clean the circuit when changing reference, following the supplier's instructions. Every new batch must be tested on a reference piece before going into production, because consistency between batches is what keeps the colour curve constant.

Effect inks (white, matt, gloss, glue or camber) are deposited in layers coordinated with the glaze and the graphics, and each one responds differently in firing. If the defect appears only where one of them acts, start the diagnosis with that one. You will find more detail in the technical guide to special effect inks.

How do the substrate, the glaze and the engobe influence printing?

The drop does not stay in the air: it lands on a surface and its behaviour depends on it. With the same ink, the same machine and the same design, a change in the substrate, the glaze or the engobe is enough for the result to change.

Absorption, moisture and surface temperature

A wet or poorly absorbent surface lets the drop spread and the outline blur. In extreme cases, the ink runs and mixes between channels. A very absorbent surface may retain the ink immediately and give less colour density. The temperature of the piece at the printer entry also matters, because a hotter piece dries the ink before it spreads. Control the residual moisture and the temperature of the piece at that point as one more process variable.

Weight, uniformity and cleanliness of the layer

A glaze applied with irregular weight changes the colour density from one area to another, and also the final shade after firing. Dust or debris on the surface prevents the ink from settling at that point and leaves uncovered areas.

Relief and flatness

On surfaces with relief, the distance between the printhead and the piece is not the same in the valley as on the crest, and the drop arrives with a different point of impact depending on the area. The result is areas with less density or with print shadows at the edges of the relief. Something similar happens with a piece that enters curved or with height differences across the width: the distance varies and definition drops in those areas. Define the print distance for the real height of the surface and check the flatness of the piece at the entry.

Glaze composition and pigment

The same pigment can develop different shades on glazes of different composition, because some glaze components react with it during firing. That is why a change of glaze requires reviewing the colour calibration, even if the ink is the same. If the defect is crazing or pinholing rather than a shade deviation, its origin usually lies in the glaze itself, and the guide to ceramic glaze defects details causes and solutions.

Why does the colour change between the printed piece and the fired piece?

What you see at the printer exit is a preview, not the result: the pigment develops its colour in the kiln. That is why a shade that drifts and a pinhole in the printed area can originate in firing.

The firing cycle

The peak temperature, the soaking time and the atmosphere of the cycle modify the final shade with the same ink and the same glaze, so each cycle needs its own calibration. When the shade drifts without anything having changed in the printing, check the kiln records before touching the curves. The glaze firing curve details how each stage affects it, and what happens to the glaze conditions what happens to the pigment.

Calibration and ink load

Colour curves or profiles relate each value of the design to a quantity of ink, and they are valid for a specific combination of ink, glaze and firing cycle. If any of the three changes, they must be recalibrated. Loading more ink than the printhead admits in order to gain intensity causes ejection failures and does not correct the shade; the limit depends on the printhead and the ink.

The eye alone is not enough to decide whether a shade is acceptable. The reference sample, the measuring conditions, the ΔE formula and the tolerance are defined once per reference, as we explain in industrial colour management.

What control routine helps prevent defects?

Most defects are detected earlier when they are always examined at the same moment and with the same criteria. The table assigns each check from the previous sections to its moment in the shift.

Moment What to check What it prevents
At the start of the shift Nozzle test pattern, ink circuit temperature and cleanliness of the cabinet Banding and lines, lack of density
After each stoppage or intervention New test pattern, condition of the nozzle plate and air in the circuit after refilling or purging Banding and lines
At each change of ink, glaze or engobe batch Test piece against the reference piece, raw and after firing Shade variations, lack of density
After replacing a printhead or a module Alignment and ejection calibration Misalignment, stitching marks
During the shift One piece at fixed intervals, observed under the same light, and glaze weight Shade variations, lack of definition
After any change to the firing cycle New colour calibration and pinhole check Shade deviations, pinholing

Save the result of each check alongside the line's change log. When a defect appears, you will be able to compare it with a history rather than with the memory of whoever was on shift, and the diagnosis in the second section will be much shorter.

At Kerafrit we develop and manufacture ceramic inkjet inks formulated for the substrate, the glaze, the printing system, the printhead and the firing cycle of each line. If you would like an ink tailored to your production, tell us your case and we will study it with you.

Featured Articles