• Products
  • Services
  • About us
  • Blog
Innovation 23 November 2026

Ceramic glaze firing curve: how it affects finish and properties

Share

When a tile comes out of the kiln with pinholes, gloss outside the target range or crazing, the first suspect is usually the glaze formulation. However, the cause may also lie in the firing cycle. The composition sets what the glaze is capable of; the curve determines what it actually delivers in the kiln.

The firing curve is the temperature profile a tile follows as it passes through the kiln. Depending on how it unfolds, the glaze melts, levels and cools in one way or another, and its gloss, texture, resistance and fit with the body depend on it.

What is a glaze firing curve and what stages does it have?

The firing curve is the record of the temperature of the piece over time. It is defined by four parameters: the heating rate, the peak temperature, the soaking time at that peak and the cooling rate. In a kiln, these parameters are distributed across its different zones.

For this reason, it is worth distinguishing between the programmed curve and the one the tile actually follows. Format, thickness and position in the kiln can make them differ, so it is advisable to measure it with a data logger that travels alongside the piece.

Drying and preheating stage

This is the stage in which residual water is removed and the organic matter in the body, the glaze and the decoration is burnt off. The ramp should be moderate: abrupt heating creates temperature differences between the centre and the edge of the piece and reduces the time available to evacuate gases.

Heating and sintering stage

The ramp speeds up to the range in which the frits begin to soften. The rate at which this stage is crossed determines the time that elapses between the onset of sintering and the melting of the glaze.

Vitrification stage: peak temperature and soaking time

These are two related variables, but they are not interchangeable. Extending the soaking time does not, on its own, make up for an insufficient peak temperature, because the viscosity of the glass changes with temperature and time only gives the glaze more margin to flow as far as that viscosity allows.

Cooling stage

In a roller kiln, three zones are distinguished: direct rapid cooling, indirect slow cooling and final rapid cooling. The slow zone coincides with the range in which the body changes volume, which is why the rate is controlled there with greater care.

What happens to the glaze at each stage of the curve?

On entering the kiln, the glaze is a layer of particles with open porosity. Through this porosity escapes the gas released by the body as carbonates and sulphates decompose, as clays lose their chemically bound water and as binders burn off. Digital decoration also adds the organic matter of the inks, which must also be evacuated.

As the temperature rises, the frits soften and the particles bond until the layer is sealed. This closure must take place once degassing has finished. If the glaze seals earlier, the gas is trapped or opens up the surface as it escapes. The margin between one phenomenon and the other depends on the melting range of the frits and on the heating ramp.

With melting, the glassy phase appears and viscosity drops. The glaze wets the surface, levels and reabsorbs some of the remaining bubbles. The fluidity reached depends on the viscosity at high temperature, which is in turn conditioned by the composition, the temperature and the time at peak.

During cooling, some compositions develop crystalline phases and the glass goes from a viscous to a rigid state. At this point the stress between the glaze and the body is fixed.

How does the curve influence gloss and texture?

In a glossy glaze, gloss depends mainly on the smoothness of the surface. With a low peak or a short soak, the layer does not level out and reflection is poorer. With a high peak or a long soak, the glaze flows excessively and loses definition.

In a matt glaze, the finish is built through crystallisation or controlled melting, so the curve decides to what extent it develops. Different cooling shifts the degree of matt and, at times, the shade as well, since the pigment interacts with the glassy phase and with the phases that crystallise.

Texture follows the same logic. Orange peel normally indicates a viscosity at high temperature that is too high for the time available, while a rough surface points to incomplete melting. When two batches of the same glaze show differences in shade or gloss, it is advisable to compare the curve records first before reviewing the formulation.

How does the curve affect resistance and other technical properties?

Resistance to abrasion, stains and chemical attack depends on the degree of melting reached, on the crystalline phases present and on the closed porosity left in the layer. A bubble close to the surface retains dirt and is the point where wear begins.

The curve also determines the fit between glaze and body. The stress between the two is fixed during cooling, and the usual aim is a glaze under slight compression. If it ends up in tension, crazing appears. If compression is excessive, edge chipping and curvature of the piece occur.

Cooling also acts on the body itself. Around 573 °C quartz changes phase and its volume varies, and cooling too fast in that range can crack the tile and alter its fit with the glaze. Finally, there is delayed crazing: over time, the body recovers moisture and expands, and a glaze that left the kiln in just the right compression ends up working in tension. In that case, cracks appear days or months after firing.

What defects appear when the curve is not right?

A curve that does not suit the glaze can lead to pinholes, bubbles, orange peel, running or crazing, among other defects. Their causes, which do not depend only on firing, are analysed in the guide to ceramic glaze defects.

How is the curve adjusted for a specific glaze?

The adjustment starts from four groups of variables. The first is the body: red or white paste and final porosity. The second, format and thickness, which determine thermal inertia and the temperature difference between the centre and the edge. The third is the application: weight, density, number of layers and digital decoration. The fourth is the kiln: length, temperature profile and atmosphere.

The work begins with the behaviour of the glaze at high temperature. The heating microscope makes it possible to follow sintering, softening and melting, and dilatometry provides information on the fit with the body. It is then tested in a laboratory kiln and, finally, in the plant. Results are checked with the tests of the UNE-EN ISO 10545 series: surface abrasion, stain resistance, chemical resistance and crazing resistance.

At Kerafrit we work with you to understand your body, your application and your cycle, and from there study the glaze that best responds to your firing conditions. Its behaviour is checked before any change is introduced into production, and subsequent follow-up between batches makes it possible to confirm that the results are maintained.

Featured Articles

  • Inicio /
  • Blog /
  • Ceramic glaze firing curve: how it affects finish and properties